80% 200 mesh mixing the ore/water grinding slurry with about 2 pounds per ton of sodium cyanide and enough quick lime to keep the pH of the solution at about At a slurry concentration of 50% solids the slurry passes through a series of agitated mixing tanks with a residence time of 24 hours